永康市龙德工具有限公司

    中文 English
发布日期:2016/11/11 点击量: 7869

 1. Cut the brick of the wheel, you must install the protective cover. Brickwork application of silicon carbide wheel, must have a factory certificate. Installation should check whether the grinding wheel cracks or moisture, to confirm qualified before use.
2. Not forced squeeze adjustment pedal leaving the cut brick grinding wheel by the load is too large; pressure, the wheel pieces easily broken. Cut the brick at the beginning, the pedal can not be pressed too heavy.
3. Cut the brick, the cut part of the width of not less than 10mm, cut brick process, shall not change the direction and location of bricks, to prevent the breakage of broken pieces of grinding wheel.
4. Cut-tiles Operators should wear protective glasses, masks and gloves.
5. Cut the brick process machinery failure, should immediately cut off the power, is strictly prohibited in the mechanical operation of the maintenance of parts cut brick machine Specifications:
1. Sawing size: 400X150X150mm 2. Spindle speed 2300r / min 3. Motor rated power 2.2kw 4. Blade diameter φ400
5. Overall dimensions 900 * 460 * 830mm 6. Machine weight 130kg The main purpose
Widely used in quality inspection of construction projects, highway engineering quality testing of common clay brick compressive test sampling to do the cutting work, can also be used for construction of special-shaped block sawing work. Cut brick use:
1, according to the size of the specimen to select the appropriate fixture, firmly stuck in the small round pillars.
2, the release of the main body of immobilization bolts suppliers Hebei Dahong Experimental Instrument Co., Ltd., turn the screw lift handle, select the required size, locking dial.
3, open the inlet valve water, put the splash cover and close the power switch, so that the grinding head rotation. 4, hand main body slowly close to the sample, began grinding, reciprocating several times.
5, loosen the small round column, grips of ingot screws, reverse installation of film prison, repeat steps 2, 3, 4, until the sample face to meet the requirements so far. Cutting the price of operating procedures 1, connected to power and water.
2, according to the size of the sample to select the appropriate fixture, the specimen clamped and transferred to the chassis center position after the clamp tight.
3, loosen the upper and lower cable tight hand wheel, turn the lift hand wheel, when the grinding wheel end face away from the specimen 1mm stop. Then tighten the cable tight on the handle, open the inlet valve water, and close the power switch, so that grinding wheel rotation, and then turn the hand wheel counterclockwise, and at the same time turn the micro-hand wheel clockwise so that the grinding head down. When the end surface of the grinding wheel contacts the sample end, the grinding head grinds until the sample end surface is polished.
4, finished grinding suppliers Hebei Dahong Experimental Instrument Co., Ltd., turn off the power and water nozzle valve and counter-clockwise rotation micro handwheel, it is in the upper limit position.

 